*Material Surface layer: BOPP Glue layer: EVA adhesive *Specification Gloss Matt *Process parameter: *Directions for usi

Send your inquiry

DESCRIPTION

Basic Info
Model NO. 1209G
Functional Layer Laminating
Packaging Carton+Pallet
Paper Core 1 Inch/2.25 Inches/3 Inches
Width 300 ~ 1800 mm
Length 300 ~ 3000 M
Thickness 18mic~35mic
Surface Gloss or Matt
Transport Package Carton Box(+Pallet If Needed)
Specification SGS RoHS
Trademark FSEKO
Origin China
HS Code 392020
Production Capacity 4500 Tons/Year
Product Description
*Material

Surface layer: BOPP
Glue layer: EVA adhesive

 

*Specification

Gloss
SPECIFICATION18mic21mic24mic24mic27mic30mic
GLOSSGLOSSGLOSSGLOSSGLOSSGLOSS
THICKNESS (mic)BASE121212151518
ADHESIVE691291212
TOTAL182124242730
WEIGHTm2/kg60.451.645.04545.4540.1136.15
kg/m20.016560.019380.02220.0220.024930.02766
WIDTH(mm)300mm-1800mm
LENGTH(m)200m-3000m
PARER CORE25mm(1inch),58mm(2.25inches),76mm(3inches)
BONDINGLESS THAN 2

Matt
SPECIFICATION24mic27mic30mic
MATTMATTMATT
THICKNESS (mic)BASE151518
ADHESIVE91212
TOTAL242730
WEIGHTm2/kg46.34137
kg/m20.02160.02440.0271
WIDTH(mm)300mm-1800mm
LENGTH(m)200m-3000m
PARER CORE25mm(1inch),58mm(2.25inches),76mm(3inches)
BONDINGLESS THAN 2

*Process parameter:

normal special
Temperature85 ~ 100ºC100 ~ 110 ºC
Roll Pressure8 ~ 15Mpa16 ~ 25 Mpa
Speed5 ~ 30 M/min5 ~10 M/min
Lamination Equipmentdry and wet laminator
RemarksSpecial laminations refer to those with thick ink, dark color, much moisture and large size paper

 

*Directions for using BOPP thermal laminating film:

Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.

*Packaging:

Standard export package with carton+pallet.